Stress corrosion cracking behaviors of FV520B stainless steel used in a failed compressor impeller
Defu Nie, Xuedong Chen, Qiaoguo Wu, Yan Liu
National Safety Engineering Technology Research Center for Pressure Vessels and Pipelines, Anhui Province Safety Technology Laboratory for Pressure Vessels and Pipelines, Hefei General Machinery Research Institute, Hefei, Anhui 230031, China
Engineering Failure Analysis, Volume 116, October 2020, 104701